This study evaluates the technical improvement achieved by applying a thick HVOF-sprayed WC-17Co interlayer between a DLC thin film and an AISI1040 steel substrate. The chemical composition (from XPS analysis) and hardness (from nano-indentation test) of the DLC films deposited on both bare and HVOF-coated AISI1040 steel are analogous. Nevertheless, the better adhesion of the DLC film on WC-17Co interlayer is demonstrated by higher critical loads recorded in scratch testing. During ball-on-disk dry sliding tribological tests, the low hardness of the AISI1040 substrate causes delamination phenomena in the DLC film. When contact pressure is low, delamination is limited, both at room temperature and at 400 degrees C; instead, delamination under high contact pressure is severe at room temperature and complete at 300 degrees C The hard. WC-17Co interlayer significantly improves the tribological performance, although delamination eventually occurs, after long sliding distances, under high contact pressure at 300 degrees C. (C) 2008 Elsevier B.V. All rights reserved.

Bolelli, G., Lusvarghi, L., Montecchi, M., Mantini, F.p., Pitacco, F., Volz, H., et al. (2008). HVOF-sprayed WC-Co as hard interlayer for DLC films. In Surface and Coatings Technology (pp.699-703). LAUSANNE : ELSEVIER SCIENCE SA [10.1016/j.surfcoat.2008.08.014].

HVOF-sprayed WC-Co as hard interlayer for DLC films

BARLETTA, MASSIMILIANO
2008-01-01

Abstract

This study evaluates the technical improvement achieved by applying a thick HVOF-sprayed WC-17Co interlayer between a DLC thin film and an AISI1040 steel substrate. The chemical composition (from XPS analysis) and hardness (from nano-indentation test) of the DLC films deposited on both bare and HVOF-coated AISI1040 steel are analogous. Nevertheless, the better adhesion of the DLC film on WC-17Co interlayer is demonstrated by higher critical loads recorded in scratch testing. During ball-on-disk dry sliding tribological tests, the low hardness of the AISI1040 substrate causes delamination phenomena in the DLC film. When contact pressure is low, delamination is limited, both at room temperature and at 400 degrees C; instead, delamination under high contact pressure is severe at room temperature and complete at 300 degrees C The hard. WC-17Co interlayer significantly improves the tribological performance, although delamination eventually occurs, after long sliding distances, under high contact pressure at 300 degrees C. (C) 2008 Elsevier B.V. All rights reserved.
35th International Conference on Metallurgical Coatings and Thin Films
San Diego, CA
APR 28-MAY 02, 2008
Amer Vacuum Soc, Adv Surf Engn Div
Rilevanza internazionale
2008
Settore ING-IND/16 - TECNOLOGIE E SISTEMI DI LAVORAZIONE
English
Ball-on-disk test; Electron Cyclotron Resonance-Chemical Vapour Deposition (ECR-CVD); High Velocity Oxygen-Fuel Spraying (HVOF); Nano-indentation; Scratch test
Intervento a convegno
Bolelli, G., Lusvarghi, L., Montecchi, M., Mantini, F.p., Pitacco, F., Volz, H., et al. (2008). HVOF-sprayed WC-Co as hard interlayer for DLC films. In Surface and Coatings Technology (pp.699-703). LAUSANNE : ELSEVIER SCIENCE SA [10.1016/j.surfcoat.2008.08.014].
Bolelli, G; Lusvarghi, L; Montecchi, M; Mantini, Fp; Pitacco, F; Volz, H; Barletta, M
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/2108/53697
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? 21
social impact