The study deals with the effects of laser surface treatments on the fatigue behavior of adhesive-bonded aluminum joints. Laser texturing, laser cleaning, and their combination are produced by adopting a 30 W nanosecond pulsed Yb:YAG laser. Parallel grooves, perpendicular to the load direction, varying in depth, width, and areal density are adopted as textured geometrical features. To assess the performance of laser treatments a central composite design (CCD) experimental plan is adopted to evaluate the apparent shear strength of single-lap joint test (ASTM D1002-10). Then, for the more promising treatment conditions, fatigue tests are carried out according to the ASTM D3166-99 standards, and cycles to failure are adopted to quantify the treatments. In addition, mechanical surface treatment (sandpaper polishing) is adopted as a reference treatment. Findings demonstrate that laser treatments significantly enhance the fatigue life of the joints (up to six times), offering a promising alternative to traditional mechanical methods.
Leone, C., Morello, D., Coscione, C., Lamanna, G., Genna, S. (2025). A preliminary study on fatigue behavior of aluminum single‐lap joints subjected to laser surface treatments. ??????? it.cilea.surplus.oa.citation.tipologie.CitationProceedings.prensentedAt ??????? Polcom 2024, Bucharest [10.1002/masy.70060].
A preliminary study on fatigue behavior of aluminum single‐lap joints subjected to laser surface treatments
Genna, Silvio
2025-01-01
Abstract
The study deals with the effects of laser surface treatments on the fatigue behavior of adhesive-bonded aluminum joints. Laser texturing, laser cleaning, and their combination are produced by adopting a 30 W nanosecond pulsed Yb:YAG laser. Parallel grooves, perpendicular to the load direction, varying in depth, width, and areal density are adopted as textured geometrical features. To assess the performance of laser treatments a central composite design (CCD) experimental plan is adopted to evaluate the apparent shear strength of single-lap joint test (ASTM D1002-10). Then, for the more promising treatment conditions, fatigue tests are carried out according to the ASTM D3166-99 standards, and cycles to failure are adopted to quantify the treatments. In addition, mechanical surface treatment (sandpaper polishing) is adopted as a reference treatment. Findings demonstrate that laser treatments significantly enhance the fatigue life of the joints (up to six times), offering a promising alternative to traditional mechanical methods.| File | Dimensione | Formato | |
|---|---|---|---|
|
26-A Preliminary Study on Fatigue Behavior of Aluminum Single‐Lap Joints Subjected to.pdf
accesso aperto
Tipologia:
Versione Editoriale (PDF)
Licenza:
Creative commons
Dimensione
3.57 MB
Formato
Adobe PDF
|
3.57 MB | Adobe PDF | Visualizza/Apri |
I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.