The aging mechanism of 10% and 30% nickel-substituted manganese hexacyanoferrate cathode material in aqueous zinc-ion batteries has been explored through the advanced synchrotron-based two-dimensional X-ray fluorescence technique. Thanks to the two-dimension modality, not only were the metal concentration dynamics throughout the entire electrodes followed during the aging process, but their spatial distribution was also revealed, suggesting the route of the material transformation. The dissolution of Mn and Ni, as well as the penetration of Zn inside the framework were detected, while the Mn aggregations were found outside the hexacyanoferrate framework. Additionally, the possibility of conducting X-ray absorption spectroscopy measurements on the regions of interest made it possible to explore the chemical state of each metal, and furthermore, synchrotron-based powder X-ray diffraction demonstrated the gradual structural modification in 30% Ni-containing sample series in terms of the different phase formation.

Maisuradze, M., Li, M., Carlomagno, I., Gaboardi, M., Aquilanti, G., Plaisier, J., et al. (2024). Aging Mechanism of Mn-Based Prussian Blue Cathode Material by Synchrotron 2D X-ray Fluorescence. BATTERIES, 10(4) [10.3390/batteries10040123].

Aging Mechanism of Mn-Based Prussian Blue Cathode Material by Synchrotron 2D X-ray Fluorescence

Mattia Gaboardi;
2024-01-01

Abstract

The aging mechanism of 10% and 30% nickel-substituted manganese hexacyanoferrate cathode material in aqueous zinc-ion batteries has been explored through the advanced synchrotron-based two-dimensional X-ray fluorescence technique. Thanks to the two-dimension modality, not only were the metal concentration dynamics throughout the entire electrodes followed during the aging process, but their spatial distribution was also revealed, suggesting the route of the material transformation. The dissolution of Mn and Ni, as well as the penetration of Zn inside the framework were detected, while the Mn aggregations were found outside the hexacyanoferrate framework. Additionally, the possibility of conducting X-ray absorption spectroscopy measurements on the regions of interest made it possible to explore the chemical state of each metal, and furthermore, synchrotron-based powder X-ray diffraction demonstrated the gradual structural modification in 30% Ni-containing sample series in terms of the different phase formation.
2024
Pubblicato
Rilevanza internazionale
Articolo
Esperti anonimi
Settore CHEM-03/A - Chimica generale e inorganica
Settore PHYS-03/A - Fisica sperimentale della materia e applicazioni
English
Con Impact Factor ISI
nickel-substituted manganese hexacyanoferrate
two-dimensional X-ray fluorescence
X-ray absorption near edge structure
X-ray diffraction
zinc-ion batteries
aqueous batteries
double-metal hexacyanoferrate
Maisuradze, M., Li, M., Carlomagno, I., Gaboardi, M., Aquilanti, G., Plaisier, J., et al. (2024). Aging Mechanism of Mn-Based Prussian Blue Cathode Material by Synchrotron 2D X-ray Fluorescence. BATTERIES, 10(4) [10.3390/batteries10040123].
Maisuradze, M; Li, M; Carlomagno, I; Gaboardi, M; Aquilanti, G; Plaisier, J; Giorgetti, M
Articolo su rivista
File in questo prodotto:
File Dimensione Formato  
batteries-10-00123-v3.pdf

accesso aperto

Tipologia: Versione Editoriale (PDF)
Licenza: Creative commons
Dimensione 4.93 MB
Formato Adobe PDF
4.93 MB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/2108/394711
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 1
  • ???jsp.display-item.citation.isi??? 1
social impact